The following observations evidence the use of Persian Cobalt (蘇麻离青) for the blue pigment. Persian cobalt was available only during the Yuan and early Ming dynasties.
- Pigment is diffused in the glaze
- Iron crystals form above areas of thick pigmentation
- Glaze surface is slightly depressed where pigment is present
- Dripping and coalescence of the pigment in line with Persian cobalt characteristics (heap and pile effect)
The following observations further support the aging commensurate with Yuan porcelains:
- Numerous brown colored bubbles within the glaze (变色氣泡). This is evident in the attached closeup picture.
- Minor surface scratches of the glaze show rainbow color diffractions, suggestive of silica crystallization (牛毛紋)
- Calcium crystallization inside large bubbles in the glaze, giving cloudy appearance
- Cloud like formations within the glaze matrix, suggestive of calcium crystallization.
The middle of the jar has a faint hairline fracture in the glaze. This is in line with Yuan dynasty jar construction as top and bottom halves were molded separately and joined in the middle.
The inside of the jar is fully glazed. As typical of Yuan ceramics. the inside surface is not smooth.
The foot of the vessel bears reddish spots, evidence of oxidation of iron in the ceramic(火石红).
Specifications
| Measurements 尺寸 | (cm) | (inch) |
|---|---|---|
| Height | 39.3 cm | 15.5 inches |
| Diameter | 34 cm | 13.4 inches |
Condition
The jar is in excellent condition with no signs of breakage or cracks. Age related crackle lines cover the entire glaze surface area.